SY-W402B
High-pressure Spray Cleaner
高压喷淋清洗剂
Silane, zirconium, phosphating, passivation, blackening and polishing systems that improve corrosion resistance and coating adhesion while replacing heavy-metal processes.
MethodSpray
TemperatureRoom temp.-80°C
Time3-10min
Bath2-10%
Overview
Silane, zirconium, phosphating, passivation, blackening and polishing systems that improve corrosion resistance and coating adhesion while replacing heavy-metal processes.
Detailed English TDS is available on request. The original Chinese product features are provided in the datasheet.
Typical process conditions
Typical parameters from the product catalog. Please validate in small batches according to substrate, equipment and line takt time.
| Method | Spray |
|---|---|
| Bath / Concentration | 2-10% |
| Temperature | Room temp.-80°C |
| Time | 3-10min |
INQUIRY & SAMPLE
Ask about SY-W402B
Tell us your substrate, current process and target performance. We can provide datasheets, samples and bath make-up advice.
- Reply within one business day
- Sample and line trial support
- Commissioning and troubleshooting